Spot of a DNA Biochip |
| SiO2 surface structured by optical lithography and coated with epoxy silane and DNA |
| SiO2 surface structured by optical lithography and coated with epoxy silane and DNA |
| SiO2 surface structured by optical lithography and coated with epoxy silane and DNA |
| |
|
|
 |
|
|
| |
|
| |
|
| |
|
|
| |
PLL-g-PEG biotin chip (3D) |
| |
| Collaboration: A. Egea, LAAS-CNRS/Innopsys and C. Vieu, LAAS-CNRS (Toulouse, France) |
|
|
| |
 |
|
| |
 |
|  | | Fast thicknesses measurement |
|
|
 |
|
|
|
|
| |
|
|
|
| |
|
|
|
| |
|
|
| |
 |
|
Protein microarray of PLL-g-PEG biotin is obtained by microcontact printing on a Standard Surf. Chips are observed and measured in air. The mean thicknesses values are around 5.7nm. |
|
 |
|
|
| |
|
|
| |
|
|
|
|
|
| |
|
|
|